Investigations of hot corrosion resistance of HVOF coated Fe based superalloy A-286 in simulated gas turbine environment SM Muthu, M Arivarasu Engineering Failure Analysis 107, 104224, 2020 | 34 | 2020 |
Electrochemical corrosion and tribological behaviour of AA6063/Si3N4/Cu (NO3) 2 composite processed using single-pass ECAPA route with 120 die angle P Sureshkumar, T Jagadeesha, L Natrayan, M Ravichandran, D Veeman, ... Journal of Materials Research and Technology 16, 715-733, 2022 | 31 | 2022 |
Investigation of hot corrosion resistance of bare and Ni-20% Cr coated superalloy 825 to Na2SO4-60% V2O5 environment at 900° C SM Muthu, M Arivarasu, N Arivazhagan Procedia Structural Integrity 14, 290-303, 2019 | 21 | 2019 |
Microstructure and High Temperature Performance of 321 SS Wall Manufactured Through Wire + Arc Additive Manufacturing S.Mohan Kumar, A.Rajesh Kannan, R.Pramod, N.Siva Shanmugam, S.M.Muthu, V ... Materials letter, 131913, 2022 | 10 | 2022 |
Improvement in hot corrosion resistance of dissimilar alloy 825 and AISI 321 CO2-laser weldment by HVOF coating in aggressive salt environment at 900°C SM Muthu, M Arivarasu, TH Krishna, S Ganguly, KVP Prabhakar, ... International Journal of Minerals, Metallurgy and Materials 27, 1536-1550, 2020 | 10 | 2020 |
Air Oxidation and Hot Corrosion Behavior of Bare and CO2 Laser-Welded Superalloy A-286 at 700 °C SM Muthu, M Arivarasu Transactions of the Indian Institute of Metals 72, 1607-1612, 2019 | 10 | 2019 |
Investigation of Air oxidation and hot corrosion behavior of Boiler grade material Austenitic stainless steel AISI 347 SM Muthu, M Venkateshkannan, S Gupta, KS Prakash, M Arivarasu, ... Materials Today: Proceedings 22, 1694-1701, 2020 | 7 | 2020 |
Hot Corrosion Studies on Dissimilar Weldments C-22 and AISI 316L in the Molten Salt K2SO4+ 60% wt NaCl Environment SM Muthu, CM Bharathi, NV Gukhan, SV Kumar, MV Kannan, M Arivarasu, ... Materials Today: Proceedings 5 (5), 13340-13346, 2018 | 7 | 2018 |
Influence of microstructure on the oxidation characteristics of conventional and wire arc additive manufactured alloy 625 at 750 ⁰C SM Muthu, MP Kumar, M Venkateshkannan, R Dinek, N Arivazhagan, ... Materials Letters 336, 133853, 2023 | 6 | 2023 |
Oxidation and hot corrosion studies on Fe-based superalloy A-286 pulsed current GTA weldments in gas turbine environment SM Muthu, M Arivarasu Materials Research Express 6 (11), 116577, 2019 | 6 | 2019 |
Oxide scale formation and damage mechanism of the alloy 625 weldments in air and simulated boiler environment under cyclic condition SM Muthu, SS Prabu, S Sujai, KD Ramkumar, N Beemkumar, ... Materials Letters 346, 134543, 2023 | 4 | 2023 |
Oxidation and Hot Corrosion Behaviour of Ni-Based Superalloy 825 and AISI 321 Dissimilar Laser Weldment in K2SO4–60% NaCl Molten Salt Environment at 650 … SM Muthu, N Arivazhagan, MN Rao, M Arivarasu Physics of Metals and Metallography 123 (13), 1306-1316, 2022 | 4 | 2022 |
Effect of addition of scandium in filler rod on tungsten inert gas welding of AA5052-H32 alloy L Nafeez Ahmed, D Veeman, SM Muthu Russian Journal of Non-Ferrous Metals 63 (3), 315-327, 2022 | 4 | 2022 |
Comparison of Hot Corrosion Performance of Bare and NiCoCrAlY-COATED Austenitic Stainless Steel Aisi 347 IN Aggressive Waste Heat Incinerator Environment at 650∘ C SM Muthu, RV Anant, D Raghul, M Ishwarya, N Arivazhagan, M Arivarasu Surface Review and Letters 27 (07), 1950168, 2020 | 4 | 2020 |
Evaluation of metallurgical and mechanical characteristics of the ferritic stainless steel AISI 430 produced by GTAW-based WAAM SM Muthu, D Veeman, A Vijayakumar, SS Prabu, S Sujai, M Arvind, ... Materials Letters 354, 135362, 2024 | 3 | 2024 |
Microstructure and hot corrosion characteristics evaluation of high-velocity oxy-fuel sprayed Ni–20%Cr coating on AISI 321 steel with Na2SO4–60%V2O5 salt … SM Muthu, M Arivarasu, BR Sanford, V Dinakaran, S Gupta Proceedings of the Institution of Mechanical Engineers, Part E: Journal of …, 2024 | 2 | 2024 |
Failure Assessment and High-Temperature Corrosion Behavior of Inconel 625 Welds in Simulated K2SO4 + 60% NaCl Boiler Environment SS Prabu, SM Muthu, S Sujai, KD Ramkumar, N Beemkumar, ... Journal of Materials Engineering and Performance 32 (24), 11024-11039, 2023 | 2 | 2023 |
Hot corrosion performance of bare and pulsed current welded Fe-based A-286 alloy in chlorine and sulphur environment MA SM Muthu, R Dinek, P Mohan, K Jithesh Proceedings of the Institution of Mechanical Engineers, Part E: Journal of …, 2022 | 2 | 2022 |
Evaluation of hot corrosion performance of HVOF coatings on PCGTA welded Fe-based alloy A-286 in Na2SO4%-7.5% NaVO3%-5% NaCl environment SM Muthu, M Arivarasu Surface Topography: Metrology and Properties 8 (4), 045021, 2020 | 2 | 2020 |
Accelerated Formation of Oxide Layers on Zircaloy-4 Utilizing Air Oxidation and Comparison with Water-Corroded Oxide Layers SM Muthu, HB Lee, BO Okonkwo, D Wang, C Jang, T Na Materials 16 (24), 7589, 2023 | 1 | 2023 |